Hickman, AR

Hot Rolled
(Produced as Black, Black Temper Passed, P&O and P&O Temper Passed)
Gauge:.052” min. – .625” min. (.500” Maximum Gauge Black Tempered Passed, .225” Maximum Gauge P&O and P&O Temper Passed)
Width: 36.00” – 64.00”;   35.50" min on P&O and P&O Temper Passed
Grades:Carbon Range C1005 – C1035, HSLA (45 – 80 (300 – 550 MPa) minimum yield, Line Pipe Grades (X42-X70), Abrasion Resistant Grades, Cooper Bearing Grades, Structural Grades 30 – 55 (210 – 380 MPa), CS, DS, A606 (Weathering Steel), Rephos/Renitrogenized, JIS and Euronorm grades


Surestride™ Floorplate
Gauge:.060” min. - .500” min.
Width:Standard 48” and 60”, inquire for special widths
Grades: CS, A36 HSLA Grade 50 (345 MPa) (minimum order quantity of 600T)


Coil Weight Restrictions
Minimum Thickness Widths
  48" 60"
>= .250 min45,000 lbs max48,000 lbs max
.150 <= .249 min44,000 lbs max48,000 lbs max
<= .149 min42,000 lbs max48,000 lbs max


Cold Rolled
Gauge:.012” min. - .130” min.
Width:35.50” – 62.50”
Grades:CS, DS, DDS, EDDS, Structural Grades 33 – 80 (230 – 550 MPa), HSLA 50 – 70 (340 – 490 MPa), Motor Lamination, A606 (Weathering Steel), Rephos/Renitrogenized, JIS and Euronorm grades


Galvanized
Gauge:.012” min. - .100” min.
Width: 35.50” – 62.50”
Grades: CS, FS, DDS, EDDS, Structural Grades 33 – 80 (230 – 550 MPa), HSLA 50 - 80 (340 - 550 MPa), DDS, EDDS, JIS and Euronorm grades
Coating Weights:G30-G235


Castrip® UCS (Ultra-thin Cast Sheet)
(Available as Black, P&O and Galvanized Sheet)
Gauge:.033” min. - .057” min.
Width:46.00” – 60.00” cut edge
Grades: CS, Structural Grades 33 - 60, HSLA Grade 50, A606 Type 4